nylon

Nylon (PA)

Polyamide filament for strong, heat-resistant functional parts. It absorbs moisture quickly, so it must be dried, and it prints best enclosed.

What it is

Nylon is the common name for polyamide (PA), a family of engineering plastics. Filaments are sold as PA6, PA11, PA12, copolymers such as Polymaker's PolyMide CoPA, and carbon or glass filled versions such as PA6-CF and PAHT-CF. They share three traits that shape the whole buying decision: strong, heat-tolerant parts, a strong appetite for water, and a tendency to warp.

Prusa's knowledge base says polyamide is hygroscopic and can absorb water weighing up to 10% of the filament's weight if stored badly. Polymaker's CoPA data sheet shows why that matters: tensile strength in the XY direction drops from 78.0 MPa dry to 34.3 MPa after the specimens were soaked to about 6% moisture.

Print settings in practice

Settings vary more than for any other common filament, so start from the data sheet for your exact product:

  • Nozzle: Bambu Lab's material table lists 260 to 300 °C (plus or minus 10 °C) for PA-CF/GF, PA6-CF/GF and PAHT-CF/GF and has no separate nozzle row for unfilled PA. Polymaker lists 250 to 270 °C for CoPA. Prusa recommends 285 °C. About 260 °C fits inside both the Bambu Lab and Polymaker ranges.
  • Bed: Bambu Lab lists 100 to 120 °C on PEI or its Engineering Plate, or 90 to 110 °C with glue stick. Prusa recommends 110 °C and its PA Nylon sheet. Polymaker is the outlier, listing 25 to 50 °C for CoPA on PC or textured PEI with glue when needed.
  • Drying: Bambu Lab marks drying as required: 80 °C for 8 to 12 hours, with desiccant during printing also required. Prusa says to dry for at least 4 hours below 90 °C. Polymaker lists 100 °C for 8 hours for CoPA and says to store and use it below 20% relative humidity.
  • Enclosure: Prusa says warping is the main disadvantage of pure polyamide and that a high ambient temperature from an enclosure helps a lot. Bambu Lab recommends an enclosed printer and does not recommend open-frame printers for PA. Polymaker says CoPA needs a closed chamber.
  • Cooling: Polymaker lists the cooling fan off for CoPA.
  • Annealing: Polymaker lists 80 °C for 6 hours for CoPA.
  • Speed and supports: Polymaker lists 50 to 200 mm/s for CoPA and names its PolyDissolve S1 as the matching support material, which helps on parts with internal overhangs.

Nozzle choice

Bambu Lab's table marks PA-CF/GF, PA6-CF/GF and PAHT-CF/GF as requiring hardened steel, with 0.6 mm marked as recommended. Prusa's composites article says carbon, glass and kevlar fibers are highly abrasive and need a hardened nozzle. Unfilled nylon can wear brass too: Polymaker says brass nozzle abrasion happens quite often with PolyMide CoPA and highly recommends a wear-resistant nozzle such as hardened steel or ruby.

Strengths and weaknesses for real projects

Nylon fits gears, hinges, clips, tool holders and brackets that see heat or repeated stress. Polymaker lists a heat deflection temperature for CoPA of 70 °C at 1.8 MPa and 111 °C at 0.45 MPa, well above the 54 °C at 0.45 MPa that Polymaker lists for its PLA-CF.

The costs are process and equipment. You need a dryer or a drying routine, a sealed storage box, an enclosure, and on many profiles a hot bed. Polymaker's CoPA data sheet also warns that self-supporting prints should have their supports removed before the material absorbs too much moisture, or the supports may bond permanently to the model.

How it compares

  • PETG-CF: Easier to keep dry and prints at 240 to 270 °C (Bambu Lab) with a 60 to 80 °C bed. Choose nylon when you need more heat resistance or wear resistance.
  • ABS and ASA: Also need an enclosure, but are less hygroscopic. Nylon is the choice for parts that flex and wear.
  • PLA-CF: Much easier to print, but Polymaker lists only 54 °C heat deflection at 0.45 MPa for its PLA-CF.
  • TPU: If you want flexibility rather than stiffness, TPU is simpler.

Which printers on this site can print it

Look for an enclosure, ideally active chamber heating, a 120 °C bed, and a hardened nozzle if you plan to print PA-CF:

  • Bambu Lab H2D: Bambu lists PA, PC and carbon or glass filled filaments, with hardened steel 350 °C nozzles, a 120 °C bed and chamber heating to 65 °C.
  • Bambu Lab X2D: hardened steel nozzles, 120 °C bed and chamber heating to 65 °C. Bambu lists fiber-filled PA6 and PAHT for the main hot end, and marks PA6-CF as "print with caution" on the auxiliary nozzle.
  • Creality K2 Plus: chamber heating to 60 °C and a hardened steel nozzle to 350 °C. Creality lists PA-CF and says PAHT-CF needs a 50 °C chamber.
  • QIDI Plus5 and QIDI Q2: 65 °C active chamber heating, a 370 °C nozzle and a 120 °C bed, which suits warp-prone nylon.
  • Prusa CORE One: enclosure with active chamber heating to 55 °C, 290 °C nozzle and 120 °C bed.

Passively enclosed printers such as the Bambu Lab P2S can print nylon, but their bed tops out at 110 °C and there is no chamber heater, so large parts are harder. See the best enclosed 3D printers and the best printers for small businesses.

Safety and ventilation

Prusa says polyamides give off a strong odor and potentially dangerous ultrafine particles (UFPs) while printing, and recommends a well-ventilated room or an enclosure. Several printers above add HEPA and activated carbon filtration. Read the safety data sheet for your specific filament.

Storage

Store nylon sealed with fresh desiccant, and print from a dry box. Bambu Lab lists desiccant during use as required for PA. If a spool has been open, dry it before printing even if it is new, since Bambu Lab's guide says moisture causes stringing, under-extrusion, holes, rough surfaces and reduced strength.

Print settings

Typenylon
BrandVarious
Nozzle / print temp260 °C
Bed temp110 °C
PriceNot listed

Pros and cons

Pros

  • High strength when kept dry
  • Heat deflection of 111 °C at 0.45 MPa (Polymaker CoPA)
  • Low friction and good abrasion resistance (Prusa)
  • Carbon and glass filled grades add dimensional stability
  • Can be annealed after printing

Cons

  • Absorbs moisture fast and must be dried
  • Warps without an enclosure
  • Strong odor and ultrafine particles while printing
  • Some guides call for a 100 to 120 °C bed
  • Wear-resistant nozzle advised; required for fiber-filled grades

Frequently asked questions

Does nylon filament need to be dried?

Yes. Bambu Lab marks drying as required for PA (80 °C for 8 to 12 hours), and Prusa says to dry for at least 4 hours below 90 °C. Prusa notes nylon can absorb up to 10% of its weight in water if stored badly.

Can I print nylon without an enclosure?

It is not recommended. Prusa calls warping the main disadvantage of pure polyamide and says an enclosure helps a lot, and Bambu Lab does not recommend open-frame printers for PA.

Do you need a hardened nozzle for nylon?

For carbon or glass filled nylon such as PA6-CF or PAHT-CF, yes: Bambu Lab's material table marks hardened steel as required. Unfilled nylon can also wear brass. Polymaker says brass nozzle abrasion happens quite often with its PolyMide CoPA and highly recommends a hardened steel or ruby nozzle.

What bed temperature does nylon need?

It depends on the product. Bambu Lab lists 100 to 120 °C (90 to 110 °C with glue stick) and Prusa recommends 110 °C, while Polymaker lists only 25 to 50 °C for PolyMide CoPA.

Are nylon printing fumes dangerous?

Prusa says polyamides give off a strong odor and potentially dangerous ultrafine particles. It recommends printing in a well-ventilated room or in an enclosure.