ASA
ASA
ASA prints much like ABS but adds high UV resistance for outdoor parts, with heat deflection around 100 °C. It still warps, needs an enclosure and gives off fumes.
What it is
ASA (acrylonitrile styrene acrylate) is often described as the outdoor version of ABS. It prints in a similar way and has similar heat resistance, but holds up much better in sunlight. Prusa's knowledge base describes ASA as having high UV resistance and calls it "suitable for outdoor use," and Polymaker's PolyLite ASA data sheet says it offers improved weather resistance compared with ABS.
Prusa lists its other strengths as good high-temperature resistance (up to 93 °C), detailed prints with no stringing, high impact and wear resistance, and easy post-processing, including acetone smoothing and gluing. The drawbacks are also familiar from ABS: significant warping, the need for an enclosure with large parts, potentially dangerous styrene fumes, high printing temperatures and partial moisture absorption.
Print settings in practice
Published ranges for ASA overlap but are not identical:
- Bambu filament guide: 240 to 280 °C nozzle, 90 to 100 °C bed on its Engineering, High Temperature and Textured PEI plates.
- Polymaker PolyLite ASA: 230 to 260 °C nozzle, 75 to 95 °C bed on PC or textured PEI, cooling fan off, 50 to 200 mm/s, and Polymaker states a chamber is needed.
- Prusa: 260 °C nozzle, 105 °C bed for the first layer and 110 °C after. Prusa says the bed should be at least 100 °C and the printer should be in an enclosure.
The 260 °C nozzle in the settings table sits in all three ranges, and the 100 °C bed matches the top of Bambu's range and Prusa's minimum. If your printer's bed tops out at 100 °C, start there; Polymaker's lower range shows some ASA grades are happy cooler.
Enclosure: treat it as required for anything but small parts. Prusa recommends an enclosure to keep the ambient temperature up, and a slicer draft shield if you have none. Keep part cooling off or low, as Polymaker specifies.
Speed: Polymaker's PolyLite ASA data sheet lists a printing speed of 50 to 200 mm/s, a much wider window than the 30 to 50 mm/s it lists for PolyLite ABS. That makes ASA a reasonable fit for the faster CoreXY printers on this site, as long as the chamber stays warm.
Nozzle: a standard nozzle is fine for unfilled ASA. Carbon or glass filled ASA blends need a hardened nozzle.
Drying: Polymaker lists 70 °C for 7 hours. Bambu's guide lists 80 °C for 8 hours in a drying oven, or 90 to 100 °C for 12 hours on an X1-series heatbed.
Strengths and weaknesses for real projects
ASA is a strong choice for parts that live outside: garden fixtures, mounts for cameras and sensors, bike and car exterior accessories, signage and replacement parts for outdoor equipment. Polymaker lists a heat deflection temperature of 100 °C at 1.8 MPa and a Vicat softening temperature of 105 °C for PolyLite ASA, so it also handles hot dashboards and summer sun.
The limits are the same as ABS. Large parts warp without a warm chamber, it needs a hot bed plus a warm chamber that open-frame budget printers lack, and the fumes mean you need ventilation. Prusa also notes partial hygroscopy, so leaving a spool out in humid air can cause trouble.
How it compares
- ABS: very similar printing behavior and heat resistance, but Prusa notes ABS lacks the UV resistance of ASA. ABS is the pick for indoor parts if you want acetone smoothing and a cheaper spool; ASA for anything outdoors.
- PETG: prints without an enclosure, and Bambu says its PETG HF resists UV, but PETG's published heat deflection (74.8 °C for Polymaker PolyLite PETG) is well below ASA. PETG is the easier outdoor option for parts that do not get very hot.
- PLA: not suited outdoors; Prusa lists low UV and temperature resistance.
Which printers on this site can print it
Look for an enclosure, a bed of at least 100 °C, and filtration. At the time of writing (October 2026), official store prices included:
- Bambu Lab P1S at $349, enclosed with an activated carbon filter; Bambu lists ASA as an ideal material.
- Elegoo Centauri Carbon 2 at $349, enclosed with a 350 °C hotend and a HEPA plus activated carbon filter.
- Bambu Lab P2S at $449, enclosed with a 110 °C bed and activated carbon filter.
- QIDI Q2 at $499, with active chamber heating and QIDI listing ASA among supported materials.
- QIDI Plus5 at $749, a larger enclosed printer with a heated chamber, a 120 °C bed and a 3-in-1 filter.
The Prusa CORE One adds a full enclosure with active chamber heating up to 55 °C. Bambu lists ASA as not recommended on the open-frame A1 and A1 mini. See our best enclosed 3D printers and the QIDI Q2 vs Bambu Lab P2S comparison.
Safety and ventilation
Prusa warns that "ASA releases potentially dangerous fumes during printing" and advises a well-ventilated area, without drafts across the print. UL Research Institutes lists ASA alongside ABS and HIPS among high-emitting filament materials, and says the VOCs released during material extrusion include known carcinogens and irritants.
Polymaker's safety data sheet for PolyLite ASA does not classify the filament itself as hazardous, but still says to "ensure good ventilation/exhaustion at the workplace" and to "use adequate ventilation to keep airborne concentrations low." An enclosed printer with a filter plus a ventilated room is the sensible setup.
Storage
Polymaker's safety data sheet says to store ASA in a cool place, in a tightly closed container, somewhere dry and well ventilated. Given Prusa's note on partial moisture absorption, keep spools sealed with desiccant and dry them before long or critical prints.
Print settings
| Type | ASA |
|---|---|
| Brand | Various |
| Nozzle / print temp | 260 °C |
| Bed temp | 100 °C |
| Price | Not listed |
Pros and cons
Pros
- High UV resistance for outdoor parts
- Heat resistant (HDT about 100 °C)
- Good impact and wear resistance
- Can be acetone smoothed and glued
- Little stringing per Prusa
Cons
- Warps significantly
- Needs an enclosure for larger parts
- Releases fumes, including styrene
- Needs a hot bed (75 to 110 °C by maker)
- Absorbs some moisture
Frequently asked questions
Is ASA better than ABS for outdoor use?
Yes. Prusa describes ASA as having high UV resistance and being suitable for outdoor use, while noting ABS lacks UV resistance and can yellow outdoors. Both print in a similar way and need an enclosure.
Does ASA need an enclosure?
For anything but small parts, yes. Prusa says the printer should be inside an enclosure with the bed at 100 °C or more, and Polymaker's data sheet states a chamber is needed.
Is it safe to print ASA indoors?
Prusa warns ASA releases potentially dangerous fumes and recommends a well-ventilated area. UL Research Institutes lists ASA among high-emitting filaments. Use an enclosed, filtered printer in a ventilated room.
What temperature should I print ASA at?
Bambu lists 240 to 280 °C, Polymaker 230 to 260 °C and Prusa 260 °C for the nozzle. Beds range from 75 to 95 °C (Polymaker) up to 105 to 110 °C (Prusa).
Can ASA be smoothed with acetone?
Yes. Prusa says ASA can be dissolved in acetone, which allows acetone smoothing and gluing. Acetone is flammable, so follow its safety instructions and work in a ventilated area.
Sources
- Prusa Knowledge Base: ASA
- Polymaker: PolyLite ASA Technical Data Sheet V5.4 (PDF)
- Polymaker: PolyLite ASA Safety Data Sheet (EU, EN, PDF)
- Bambu Lab: Bambu Filament Guide (PDF)
- UL Research Institutes: Comprehensive Emissions Data from Material Extrusion 3D Printing Now Available (Dec 2023)
- Prusa Knowledge Base: ABS
- Polymaker: PolyLite ABS Technical Data Sheet V5.2 (PDF)
- Polymaker: PolyLite PETG Technical Data Sheet V5.2 (PDF)